Title: | Wear resistance of austempered pearlitic ductile iron | Authors: | Ješić, Dušan Kovač, P. Plavšić, M. Šooš L. Sarjanovic D. |
Issue Date: | 1-Jan-2018 | Journal: | Kovove Materialy | Abstract: | © 2018 Kovove Materialy. All rights reserved. The influence of austempering temperature on tribological properties of austempered pearlitic ductile iron (ADI) was investigated. The as-cast ductile iron was subjected to heat treatments consisting of austenitization at 900°C followed by austempering at temperatures of 250, 300 and 350°C for 120 min. The austempered samples were subjected to abrasion and adhesion wear resistance tests using steel and ductile iron plates. The abrasive wear testing of the tribo-pair was undertaken with the sanding plate. The results of abrasion and adhesion wear resistance tests are presented, and the effect of austempering temperature is discussed. | URI: | https://open.uns.ac.rs/handle/123456789/2258 | ISSN: | 0023432X | DOI: | 10.4149/km-2018-6-415 |
Appears in Collections: | Naučne i umetničke publikacije |
Show full item record
SCOPUSTM
Citations
2
checked on Nov 20, 2023
Page view(s)
18
Last Week
17
17
Last month
0
0
checked on May 3, 2024
Google ScholarTM
Check
Altmetric
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.