Title: Wear resistance of austempered pearlitic ductile iron
Authors: Ješić, Dušan
Kovač, P.
Plavšić, M.
Šooš L.
Sarjanovic D.
Issue Date: 1-Jan-2018
Journal: Kovove Materialy
Abstract: © 2018 Kovove Materialy. All rights reserved. The influence of austempering temperature on tribological properties of austempered pearlitic ductile iron (ADI) was investigated. The as-cast ductile iron was subjected to heat treatments consisting of austenitization at 900°C followed by austempering at temperatures of 250, 300 and 350°C for 120 min. The austempered samples were subjected to abrasion and adhesion wear resistance tests using steel and ductile iron plates. The abrasive wear testing of the tribo-pair was undertaken with the sanding plate. The results of abrasion and adhesion wear resistance tests are presented, and the effect of austempering temperature is discussed.
URI: https://open.uns.ac.rs/handle/123456789/2258
ISSN: 0023432X
DOI: 10.4149/km-2018-6-415
Appears in Collections:Naučne i umetničke publikacije

Show full item record

SCOPUSTM   
Citations

2
checked on Nov 20, 2023

Page view(s)

18
Last Week
17
Last month
0
checked on May 3, 2024

Google ScholarTM

Check

Altmetric


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.