Nаziv: Improved ejection test for evaluation of soldering tendency of cast alloy to die core materials
Аutоri: Terek, Pal 
Kovačević, Lazar 
Miletić, Aleksandar
Kukuruzović, Dragan 
Baloš, Sebastian 
Škorić, Branko 
Dаtum izdаvаnjа: 1-апр-2019
Čаsоpis: Journal of Materials Processing Technology
Sažetak: © 2018 Elsevier B.V. Cast alloy soldering is a serious issue of a modern high pressure die casting (HPDC) industry. It endangers the die integrity, affects the casting quality and causes considerable production downtime, which altogether raise production costs. Development of new soldering resistant materials and coatings for HPDC dies is a promising approach in a struggle for the reduction of soldering effects. Performance of new materials for such application is most appropriately evaluated by laboratory tests. One of the tests is the ejection test in which a force required to eject a pin sample from a casting presents a measure of the cast alloy soldering tendency. In this paper, comparison between two currently used and one newly proposed method for the production of pin-casting assemblies is presented. For this purpose, pins made of X27CrMoV51 steel, and Al–Si–Cu cast alloy were used. The ejections of the pin samples were carried out on tensile testing machines, and force displacement diagrams were recorded. After the ejections, casting and pin surfaces were visually examined. The employed casting methods were numerically simulated. For the methods used so far, it was found that uniformity of a pin-casting contact is disrupted by the presence of shrinkage cavities, oxide films, and sinking-in of the casting surfaces. These imperfections formed due to inadequate casting filling and solidification conditions. On the other side, the newly designed method resulted in a uniform and a high-quality pin-casting contact, obtained through a casting process characterized with more severe soldering conditions. Consequently, for new method the recorded force and work of the ejection force are significantly higher and the cast alloy is evenly distributed on pin surfaces. New method more realistically replicates the conditions that exist between paired materials in real HPDC process. It is also simple for use and results are repeatable with a reasonable scatter.
URI: https://open.uns.ac.rs/handle/123456789/389
ISSN: 9240136
DOI: 10.1016/j.jmatprotec.2018.10.038
Nаlаzi sе u kоlеkciјаmа:FTN Publikacije/Publications

Prikаzаti cеlоkupаn zаpis stаvki

SCOPUSTM   
Nаvоđеnjа

3
prоvеrеnо 29.04.2023.

Prеglеd/i stаnicа

31
Prоtеklа nеdеljа
9
Prоtеkli mеsеc
4
prоvеrеnо 10.05.2024.

Google ScholarTM

Prоvеritе

Аlt mеtrikа


Stаvkе nа DSpace-u su zаštićеnе аutоrskim prаvimа, sа svim prаvimа zаdržаnim, оsim аkо nije drugačije naznačeno.