Nаziv: | Composites based on waste rubber powder and rubber blends: BR/CSM | Аutоri: | Marković G. Veljković O. Marinović-Cincović M. Jovanović V. Samaržija-Jovanović S. Budinski-Simendić, Jaroslava |
Dаtum izdаvаnjа: | 1-феб-2013 | Čаsоpis: | Composites Part B: Engineering | Sažetak: | Blend of polybutadiene (BR) rubber with varying ratios of chlorosulphonated polyethylene rubber (CSM), BR/CSM, keeping the total waste rubber powder (WRP) content constant at 50 phr (parts per 100 rubber) have been prepared on a laboratory-size (300 × 600 mm) two-roll mixing mill maintained at 40 ± 5 °C. The mechanical properties, namely tensile strength (TS), tensile modulus at 100% elongation (M100), elongation at break (Eb%) and hardness have been followed up as a function of irradiation dose (dose rate of 10 kGy h-1 and total absorbed dose of 100, 200, 300 and 400 kGy) as well as blend composition. The results indicated that the addition of CSM has improved the properties of BR/CSM rubber blends waste rubber powder filled composites. The improvement in mechanical properties of the BR/CSM/WRP (50/50/50) rubber blends is in correlation with homogenous WRP distribution which has been assigned by scanning electron microscopy. Also BR/CSM rubber blends waste rubber powder filled composites are thermally and irradiation more stable than BR and CSM rubbers alone. © 2012 Elsevier Ltd. All rights reserved. | URI: | https://open.uns.ac.rs/handle/123456789/13012 | ISSN: | 13598368 | DOI: | 10.1016/j.compositesb.2012.08.013 |
Nаlаzi sе u kоlеkciјаmа: | TF Publikacije/Publications |
Prikаzаti cеlоkupаn zаpis stаvki
SCOPUSTM
Nаvоđеnjа
33
prоvеrеnо 03.05.2024.
Prеglеd/i stаnicа
27
Prоtеklа nеdеljа
13
13
Prоtеkli mеsеc
0
0
prоvеrеnо 10.05.2024.
Google ScholarTM
Prоvеritе
Аlt mеtrikа
Stаvkе nа DSpace-u su zаštićеnе аutоrskim prаvimа, sа svim prаvimа zаdržаnim, оsim аkо nije drugačije naznačeno.